Refractory
brown fused alumina for refractory material
brown fused alumina is good raw material for castable refractory, ceramic refractory
brown fused alumina character:brown fused alumina is fused and crystallized under high temperature from a mixture of bauxite and other materials. It is characterized by its high...
brown fused alumina for refractory material
brown fused alumina is good raw material for castable refractory, it has high density. strong hardness.
brown fused alumina character:brown fused alumina is fused and crystallized under high temperature from a mixture of bauxite and other materials. It is characterized...
synthetic slag for steel refine
synthetic slag is good metallugyl flux. it shorten the metal melting time, and protect steel laddle
synthetic slag application .1) Uniform composition, low melting point slag minerals (≤ 1350 ), melting fast, melting time shortened, slag forming fast, and reducing dust...
slag conditioner for laddle
synthetic slag is good metallugyl flux. it shorten the metal melting time, and protect steel laddle
synthetic slag application .1) Uniform composition, low melting point slag minerals (≤ 1350 ), melting fast, melting time shortened, slag forming fast, and reducing dust...
calcium aluminate /synthetic slag
synthetic slag is good metallugyl flux. it shorten the metal melting time, and protect steel laddle
synthetic slag application .1) Uniform composition, low melting point slag minerals (≤ 1350 ), melting fast, melting time shortened, slag forming fast, and reducing dust...
synthetic slag /calcium aluminate for steel refine
synthetic slag is good metallugyl flux. it shorten the metal melting time, and protect steel laddle